Registration Dossier

Administrative data

Endpoint:
stability: thermal, sunlight, metals, other
Remarks:
Migrated from section 'Stability: thermal, sunlight, metals'
Type of information:
experimental study
Adequacy of study:
supporting study
Reliability:
2 (reliable with restrictions)
Rationale for reliability incl. deficiencies:
other: scientifically acceptable

Data source

Reference
Reference Type:
study report
Title:
Unnamed
Year:
1978
Report Date:
1978

Materials and methods

Principles of method if other than guideline:
other: measured (DTA)
GLP compliance:
no

Test material

Reference
Name:
Unnamed
Type:
Constituent
Details on test material:
Name of test material (as cited in study report): acrylic acid, monoester with propane-1,2-diol
Analytical purity: pure

Results and discussion

For thermal stability study

Test substance thermally stable:
no
Operating temperature
Operating temp.:
30 - 460 °C

Any other information on results incl. tables

1. exothermal reaction

onset: 180 °C

maximum 210 °C

energy release: 370 J/g

2. exothermal reaction

onset: 300 °C

maximum: 355 °C

energy release: 180 J/g