Registration Dossier

Diss Factsheets

Administrative data

Endpoint:
relative density
Remarks:
Other density types indicated (migrated information): density
Type of information:
experimental study
Adequacy of study:
key study
Study period:
03 January 2012- 19 March 2012
Reliability:
1 (reliable without restriction)
Rationale for reliability incl. deficiencies:
other: The study has been performed according to OECD and EC guidelines and according to the principles of GLP.

Data source

Reference
Reference Type:
study report
Title:
Unnamed
Year:
2012
Report date:
2012

Materials and methods

Test guidelineopen allclose all
Qualifier:
according to guideline
Guideline:
EU Method A.3 (Relative Density)
Version / remarks:
(2008)
Deviations:
no
Qualifier:
according to guideline
Guideline:
OECD Guideline 109 (Density of Liquids and Solids)
Version / remarks:
(1995)
Deviations:
no
GLP compliance:
yes (incl. QA statement)
Type of method:
other: Helium gas comparison pycnometer (for solids)

Test material

Constituent 1
Details on test material:
- Physical state: Clear colourless/slightly yellow, sticky resin
- Stability under test conditions: Stable
- Storage condition of test material: At room temperature protected from light
- Stability at higher temperatures: Maximum 1 month at 50°C
- General information: Avoid heat, direct sunlight, acid and base

Results and discussion

Densityopen allclose all
Type:
density
Density:
1.19 g/cm³
Temp.:
20 °C
Type:
relative density
Density:
1.19
Temp.:
20 °C
Remarks on result:
other: D4(20)

Any other information on results incl. tables

Individual measurements: 1.187 and 1.188 g/cm3 . Accuracy is < 0.02 g/cm3 .

Table: Calibration values

     

 

[cm3]

criteria

 

 

 

Reference volume

23.21

23.41 ± 0.23 cm3

Sample chamber volume

41.87

41.91 ± 0.42 cm3

Vessel volume

6.22

6.26 ± 0.06 cm3

     

 

Applicant's summary and conclusion

Conclusions:
Density of the test substance at 20ºC: 1.19 g/cm3
Relative density (D4(20)): 1.19